General
Property | Value | Comment |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Charpy impact energy | 41.0 J Show Material materials with Charpy impact energy of 41.0 J | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging | |
Elastic modulus | 190.0 - 210.0 GPa Show Material materials with Elastic modulus of 190.0 - 210.0 GPa | Typical for Steel | |||
Hardness, Brinell | 149.0 - 207.0 [-] Show Material materials with Hardness, Brinell of 149.0 - 207.0 [-] | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging | |
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel | |||
Reduction of area | 40.0 % Show Material materials with Reduction of area of 40.0 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging | |
Tensile strength | 415.0 MPa Show Material materials with Tensile strength of 415.0 MPa | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.2 Show Material materials with Carbon of 0.2 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Chromium | 1.5 - 2.0 % Show Material materials with Chromium of 1.5 - 2.0 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Copper | 0.4 Show Material materials with Copper of 0.4 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Manganese | 0.2 - 0.4 % Show Material materials with Manganese of 0.2 - 0.4 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Molybdenum | 0.4 - 0.6 % Show Material materials with Molybdenum of 0.4 - 0.6 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Nickel | 2.8 - 3.9 % Show Material materials with Nickel of 2.8 - 3.9 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Niobium | 0.02 Show Material materials with Niobium of 0.02 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Phosphorus | 0.02 Show Material materials with Phosphorus of 0.02 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Silicon | 0.35 Show Material materials with Silicon of 0.35 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Sulfur | 0.02 Show Material materials with Sulfur of 0.02 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Vanadium | 0.05 Show Material materials with Vanadium of 0.05 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |