Elongation A50 A50
0 - 20 % at 20 °C
Hardness, Brinell HB
0 - 217 [-] at 20 °C
Hardness, Rockwell B HRB
0 - 95 [-] at 20 °C
Tensile strength Rm
0 - 415 MPa at 20 °C
Yield strength YS
0 - 240 MPa at 20 °C
Element
Weight %
Comment
17.5 - 19.5 %
1.75 - 2.5 %
0 - 0.03 %
0 - 1 %
0 - 1 %