This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.
Density ρ
7.9 - 8.2 g/cm³ at 20 °C
Typical for Austenitic Stainless Steel
Poisson's ratio ν
0.3 [-] at 20 °C
Typical for Austenitic Stainless Steel
Tensile strength Rm
0 - 690 MPa at 20 °C
Yield strength YS
0 - 380 MPa at 20 °C
Coefficient of thermal expansion α
1.7E-5 - 1.9E-5 1/K at 20 °C
Typical for Austenitic Stainless Steel
Melting point Tm
1375 - 1450 °C
Typical for Austenitic Stainless Steel
Thermal conductivity λ
11 - 21 W/(m·K) at 20 °C
Typical for Austenitic Stainless Steel
Element
Weight %
Comment
20.5 - 23.5 %
11.5 - 13.5 %
4 - 6 %
1.5 - 3 %
0.2 - 0.4 %
This material data has been provided by ASTM.