Mechanical

PropertyTemperatureValue

Elongation A50

23.0 °C

15 %

Show Material materials with Elongation A50 of 15 %

Reduction of area

23.0 °C

45 %

Show Material materials with Reduction of area of 45 %

Tensile strength

23.0 °C

585 MPa

Show Material materials with Tensile strength of 585 MPa

Yield strength

23.0 °C

415 MPa

Show Material materials with Yield strength of 415 MPa

Chemical properties

PropertyValue

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Chromium

1 - 1.5 %

Show Material materials with Chromium of 1 - 1.5 %

Manganese

0.5 - 0.9 %

Show Material materials with Manganese of 0.5 - 0.9 %

Molybdenum

0.9 - 1.2 %

Show Material materials with Molybdenum of 0.9 - 1.2 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.2 - 0.6 %

Show Material materials with Silicon of 0.2 - 0.6 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Vanadium

0.2 - 0.35 %

Show Material materials with Vanadium of 0.2 - 0.35 %