General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 14 J Show Material materials with Charpy impact energy of 14 J | |
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 23.0 °C | 760 MPa Show Material materials with Tensile strength of 760 MPa | |
Yield strength | 23.0 °C | 590 MPa Show Material materials with Yield strength of 590 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 % Show Material materials with Aluminium of 0.25 % |
Carbon | 0.1 % Show Material materials with Carbon of 0.1 % |
Chromium | 58 - 62 % Show Material materials with Chromium of 58 - 62 % |
Iron | 1 % Show Material materials with Iron of 1 % |
Manganese | 0.3 % Show Material materials with Manganese of 0.3 % |
Nitrogen | 0.3 % Show Material materials with Nitrogen of 0.3 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |
Titanium | 0.5 % Show Material materials with Titanium of 0.5 % |