General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Vanadium Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Chromium Vanadium Steel |
Elongation A50 | 23.0 °C | 22 % Show Material materials with Elongation A50 of 22 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Chromium Vanadium Steel |
Tensile strength | 23.0 °C | 586 MPa Show Material materials with Tensile strength of 586 MPa | |
Yield strength | 23.0 °C | 379 MPa Show Material materials with Yield strength of 379 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K | Typical for Chromium Vanadium Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Chromium Vanadium Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.3 % Show Material materials with Carbon of 0.3 % |
Manganese | 0.7 - 1 % Show Material materials with Manganese of 0.7 - 1 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 0.2 - 0.8 % Show Material materials with Silicon of 0.2 - 0.8 % |
Sulfur | 0.045 % Show Material materials with Sulfur of 0.045 % |
Vanadium | 0.05 - 0.15 % Show Material materials with Vanadium of 0.05 - 0.15 % |