Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 41 J Show Material materials with Charpy impact energy of 41 J | |
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 22 % Show Material materials with Elongation A50 of 22 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 40 % Show Material materials with Reduction of area of 40 % | |
Tensile strength | 23.0 °C | 620 MPa Show Material materials with Tensile strength of 620 MPa | |
Yield strength Rp0.2 | 23.0 °C | 450 MPa Show Material materials with Yield strength Rp0.2 of 450 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.22 % Show Material materials with Carbon of 0.22 % |
Chromium | 1.35 - 1.85 % Show Material materials with Chromium of 1.35 - 1.85 % |
Manganese | 0.5 - 0.8 % Show Material materials with Manganese of 0.5 - 0.8 % |
Molybdenum | 0.35 - 0.6 % Show Material materials with Molybdenum of 0.35 - 0.6 % |
Nickel | 2.5 - 3.5 % Show Material materials with Nickel of 2.5 - 3.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.6 % Show Material materials with Silicon of 0.6 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |