General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 41 J Show Material materials with Charpy impact energy of 41 J | |
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 18 % Show Material materials with Elongation A50 of 18 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 35 % Show Material materials with Reduction of area of 35 % | |
Tensile strength | 23.0 °C | 620 MPa Show Material materials with Tensile strength of 620 MPa | |
Yield strength Rp0.2 | 23.0 °C | 485 MPa Show Material materials with Yield strength Rp0.2 of 485 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.2 % Show Material materials with Carbon of 0.2 % |
Chromium | 1.5 - 2 % Show Material materials with Chromium of 1.5 - 2 % |
Manganese | 0.4 - 0.7 % Show Material materials with Manganese of 0.4 - 0.7 % |
Molybdenum | 0.4 - 0.6 % Show Material materials with Molybdenum of 0.4 - 0.6 % |
Nickel | 2.75 - 3.9 % Show Material materials with Nickel of 2.75 - 3.9 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.6 % Show Material materials with Silicon of 0.6 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |