Density ρ
7.9 - 8.2 g/cm³ at 20 °C
Typical for Austenitic Stainless Steel
Elongation A50 A50
0 - 40 % at 20 °C
Hardness, Brinell HB
0 - 217 [-] at 20 °C
Hardness, Rockwell B HRB
0 - 95 [-] at 20 °C
Poisson's ratio ν
0.3 [-] at 20 °C
Typical for Austenitic Stainless Steel
Tensile strength Rm
0 - 515 MPa at 20 °C
Yield strength YS
0 - 260 MPa at 20 °C
Coefficient of thermal expansion α
1.7E-5 - 1.9E-5 1/K at 20 °C
Typical for Austenitic Stainless Steel
Melting point Tm
1375 - 1450 °C
Typical for Austenitic Stainless Steel
Thermal conductivity λ
11 - 21 W/(m·K) at 20 °C
Typical for Austenitic Stainless Steel
Element
Weight %
Comment
16 - 18 %
5.5 - 7.5 %
3.5 - 5.5 %
0 - 0.15 %
0 - 0.06 %
This material data has been provided by ASTM.