General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Nickel Molybdenum Steel |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Tensile strength | 23.0 °C | 630 MPa Show Material materials with Tensile strength of 630 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 9E-6 - 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 9E-6 - 1.3E-5 1/K | Typical for Nickel Molybdenum Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel | |
Specific heat capacity | 23.0 °C | 335 - 481 J/(kg·K) Show Material materials with Specific heat capacity of 335 - 481 J/(kg·K) | Typical for Nickel Molybdenum Steel |
Thermal conductivity | 23.0 °C | 44 W/(m·K) Show Material materials with Thermal conductivity of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.13 - 0.18 % Show Material materials with Carbon of 0.13 - 0.18 % |
Chromium | 0.2 % Show Material materials with Chromium of 0.2 % |
Copper | 0.35 % Show Material materials with Copper of 0.35 % |
Manganese | 0.4 - 0.6 % Show Material materials with Manganese of 0.4 - 0.6 % |
Molybdenum | 0.2 - 0.3 % Show Material materials with Molybdenum of 0.2 - 0.3 % |
Nickel | 3.25 - 3.75 % Show Material materials with Nickel of 3.25 - 3.75 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % |
Sulfur | 0.04 % Show Material materials with Sulfur of 0.04 % |