General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ at 23.0 °C | 23.0 °C | Typical for Steel |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa at 23.0 °C | 23.0 °C | Typical for Steel |
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] at 23.0 °C | 23.0 °C | Typical for Steel |
Tensile strength | 770 MPa Show Material materials with Tensile strength of 770 MPa at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Carbon | 0.51 - 0.59 % | |
Chromium | 0.6 - 0.8 % | |
Copper | 0.35 % | |
Manganese | 0.6 - 0.8 % | |
Molybdenum | 0.06 % | |
Nickel | 0.25 % | |
Phosphorus | 0.04 % | |
Silicon | 1.2 - 1.6 % | |
Sulfur | 0.04 % |