General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.9 - 8.2 g/cm³ Show Material materials with Density of 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 195 GPa Show Material materials with Elastic modulus of 195 GPa | Typical for Austenitic Stainless Steel |
Elongation A50 | 23.0 °C | 40 % Show Material materials with Elongation A50 of 40 % | |
Hardness, Brinell | 23.0 °C | 201 [-] Show Material materials with Hardness, Brinell of 201 [-] | |
Hardness, Rockwell B | 23.0 °C | 92 [-] Show Material materials with Hardness, Rockwell B of 92 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Austenitic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Austenitic Stainless Steel |
Tensile strength | 23.0 °C | 515 MPa Show Material materials with Tensile strength of 515 MPa | |
Yield strength | 23.0 °C | 205 MPa Show Material materials with Yield strength of 205 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Melting point | 1230 - 1480 °C Show Material materials with Melting point of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Specific heat capacity | 23.0 °C | 440 J/(kg·K) Show Material materials with Specific heat capacity of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Thermal conductivity | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Thermal conductivity of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Electrical resistivity of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |