ASTM A204 Grade B As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A200

20.0 °C

17 %

Show Material materials with Elongation A200 of 17 %

Elongation A50

20.0 °C

21 %

Show Material materials with Elongation A50 of 21 %

Tensile strength

20.0 °C

485 - 620 MPa

Show Material materials with Tensile strength of 485 - 620 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

275 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 275 MPa

Chemical properties

PropertyValue

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Manganese

0.9 %

Show Material materials with Manganese of 0.9 %

Molybdenum

0.45 - 0.6 %

Show Material materials with Molybdenum of 0.45 - 0.6 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.15 - 0.4 %

Show Material materials with Silicon of 0.15 - 0.4 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %