Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 23.0 °C | 14 - 16 % Show Material materials with Elongation A50 of 14 - 16 % |
Reduction of area | 23.0 °C | 45 % Show Material materials with Reduction of area of 45 % |
Tensile strength | 23.0 °C | 725 - 930 MPa Show Material materials with Tensile strength of 725 - 930 MPa |
Yield strength | 23.0 °C | 620 - 690 MPa Show Material materials with Yield strength of 620 - 690 MPa |
Chemical properties
Property | Value |
---|---|
Boron | 2.5E-3 % Show Material materials with Boron of 2.5E-3 % |
Carbon | 0.15 - 0.21 % Show Material materials with Carbon of 0.15 - 0.21 % |
Chromium | 0.5 - 0.8 % Show Material materials with Chromium of 0.5 - 0.8 % |
Manganese | 0.8 - 1.1 % Show Material materials with Manganese of 0.8 - 1.1 % |
Molybdenum | 0.18 - 0.28 % Show Material materials with Molybdenum of 0.18 - 0.28 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.4 - 0.8 % Show Material materials with Silicon of 0.4 - 0.8 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Zirconium | 0.05 - 0.15 % Show Material materials with Zirconium of 0.05 - 0.15 % |