Mechanical
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Reduction of area | 45 % Show Material materials with Reduction of area of 45 % | Quenched and Tempered | ASTM A517 | Plate |
Tensile strength | 725 - 930 MPa Show Material materials with Tensile strength of 725 - 930 MPa | Quenched and Tempered | ASTM A517 | Plate |
795 - 930 MPa Show Material materials with Tensile strength of 795 - 930 MPa | Quenched and Tempered | ASTM A517 | Plate | |
Yield strength | 620 MPa Show Material materials with Yield strength of 620 MPa | Quenched and Tempered | ASTM A517 | Plate |
690 MPa Show Material materials with Yield strength of 690 MPa | Quenched and Tempered | ASTM A517 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Boron | 0.0005 - 0.005 % Show Material materials with Boron of 0.0005 - 0.005 % | Quenched and Tempered | ASTM A517 | Plate |
Carbon | 0.15 - 0.21 % Show Material materials with Carbon of 0.15 - 0.21 % | Quenched and Tempered | ASTM A517 | Plate |
Chromium | 0.4 - 0.65 % Show Material materials with Chromium of 0.4 - 0.65 % | Quenched and Tempered | ASTM A517 | Plate |
Manganese | 0.7 - 1 % Show Material materials with Manganese of 0.7 - 1 % | Quenched and Tempered | ASTM A517 | Plate |
Molybdenum | 0.15 - 0.25 % Show Material materials with Molybdenum of 0.15 - 0.25 % | Quenched and Tempered | ASTM A517 | Plate |
Phosphorus | 0.025 % Show Material materials with Phosphorus of 0.025 % | Quenched and Tempered | ASTM A517 | Plate |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % | Quenched and Tempered | ASTM A517 | Plate |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % | Quenched and Tempered | ASTM A517 | Plate |
Titanium | 0.01 - 0.04 % Show Material materials with Titanium of 0.01 - 0.04 % | Quenched and Tempered | ASTM A517 | Plate |
Vanadium | 0.03 - 0.08 % Show Material materials with Vanadium of 0.03 - 0.08 % | Quenched and Tempered | ASTM A517 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |