General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 14 - 16 % Show Material materials with Elongation A50 of 14 - 16 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 45 % Show Material materials with Reduction of area of 45 % | |
Tensile strength | 23.0 °C | 725 - 930 MPa Show Material materials with Tensile strength of 725 - 930 MPa | |
Yield strength | 23.0 °C | 620 - 690 MPa Show Material materials with Yield strength of 620 - 690 MPa |
Chemical properties
Property | Value |
---|---|
Boron | 1E-3 - 5E-3 % Show Material materials with Boron of 1E-3 - 5E-3 % |
Carbon | 0.12 - 0.2 % Show Material materials with Carbon of 0.12 - 0.2 % |
Chromium | 1.4 - 2 % Show Material materials with Chromium of 1.4 - 2 % |
Manganese | 0.4 - 0.7 % Show Material materials with Manganese of 0.4 - 0.7 % |
Molybdenum | 0.4 - 0.6 % Show Material materials with Molybdenum of 0.4 - 0.6 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.1 - 0.4 % Show Material materials with Silicon of 0.1 - 0.4 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Titanium | 0.01 - 0.1 % Show Material materials with Titanium of 0.01 - 0.1 % |