General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Medium Carbon Steel |
Elongation A50 | 23.0 °C | 16 % Show Material materials with Elongation A50 of 16 % | |
Hardness, Brinell | 23.0 °C | 223 - 277 [-] Show Material materials with Hardness, Brinell of 223 - 277 [-] | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Medium Carbon Steel |
Reduction of area | 23.0 °C | 32 % Show Material materials with Reduction of area of 32 % | |
Shear modulus | 23.0 °C | 75 - 80 GPa Show Material materials with Shear modulus of 75 - 80 GPa | Typical for Carbon Steel |
Tensile strength | 23.0 °C | 760 MPa Show Material materials with Tensile strength of 760 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.32E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Max service temperature | 500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1380 - 1514 °C Show Material materials with Melting point of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Specific heat capacity | 23.0 °C | 470 - 520 J/(kg·K) Show Material materials with Specific heat capacity of 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Thermal conductivity | 23.0 °C | 21 - 52 W/(m·K) Show Material materials with Thermal conductivity of 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.06 % Show Material materials with Aluminium of 0.06 % |
Carbon | 0.5 - 0.65 % Show Material materials with Carbon of 0.5 - 0.65 % |
Chromium | 0.25 % Show Material materials with Chromium of 0.25 % |
Copper | 0.35 % Show Material materials with Copper of 0.35 % |
Manganese | 0.6 - 0.9 % Show Material materials with Manganese of 0.6 - 0.9 % |
Molybdenum | 0.1 % Show Material materials with Molybdenum of 0.1 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 1 % Show Material materials with Silicon of 0.15 - 1 % |
Sulfur | 0.005 - 0.04 % Show Material materials with Sulfur of 0.005 - 0.04 % |
Titanium | 0.03 % Show Material materials with Titanium of 0.03 % |
Vanadium | 0.04 % Show Material materials with Vanadium of 0.04 % |