Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 23.0 °C | 27 - 34 J Show Material materials with Charpy impact energy of 27 - 34 J |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % |
Tensile strength | 23.0 °C | 655 - 795 MPa Show Material materials with Tensile strength of 655 - 795 MPa |
Yield strength Rp0.2 | 23.0 °C | 450 MPa Show Material materials with Yield strength Rp0.2 of 450 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 - 0.12 % Show Material materials with Aluminium of 0.02 - 0.12 % |
Carbon | 0.13 % Show Material materials with Carbon of 0.13 % |
Manganese | 0.3 - 0.6 % Show Material materials with Manganese of 0.3 - 0.6 % |
Molybdenum | 0.2 - 0.35 % Show Material materials with Molybdenum of 0.2 - 0.35 % |
Nickel | 4.8 - 5.2 % Show Material materials with Nickel of 4.8 - 5.2 % |
Nitrogen | 0.02 % Show Material materials with Nitrogen of 0.02 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.2 - 0.4 % Show Material materials with Silicon of 0.2 - 0.4 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |