Mechanical
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Charpy impact energy | 27 J Show Material materials with Charpy impact energy of 27 J | Heat-Treated | ASTM A738 | Plate |
Tensile strength | 485 - 620 MPa Show Material materials with Tensile strength of 485 - 620 MPa | Heat-Treated | ASTM A738 | Plate |
515 - 655 MPa Show Material materials with Tensile strength of 515 - 655 MPa | Heat-Treated | ASTM A738 | Plate | |
550 - 690 MPa Show Material materials with Tensile strength of 550 - 690 MPa | Heat-Treated | ASTM A738 | Plate | |
Yield strength | 315 MPa Show Material materials with Yield strength of 315 MPa | Heat-Treated | ASTM A738 | Plate |
380 MPa Show Material materials with Yield strength of 380 MPa | Heat-Treated | ASTM A738 | Plate | |
415 MPa Show Material materials with Yield strength of 415 MPa | Heat-Treated | ASTM A738 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.2 % Show Material materials with Carbon of 0.2 % | Heat-Treated | ASTM A738 | Plate |
Chromium | 0.25 % Show Material materials with Chromium of 0.25 % | Heat-Treated | ASTM A738 | Plate |
Copper | 0.35 % Show Material materials with Copper of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % | Heat-Treated | ASTM A738 | Plate |
Molybdenum | 0.08 % Show Material materials with Molybdenum of 0.08 % | Heat-Treated | ASTM A738 | Plate |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % | Heat-Treated | ASTM A738 | Plate |
Phosphorus | 0.025 % Show Material materials with Phosphorus of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Silicon | 0.15 - 0.5 % Show Material materials with Silicon of 0.15 - 0.5 % | Heat-Treated | ASTM A738 | Plate |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % | Heat-Treated | ASTM A738 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |