Mechanical
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Charpy impact energy | 27 J Show Material materials with Charpy impact energy of 27 J | Heat-Treated | ASTM A738 | Plate |
Tensile strength | 585 - 724 MPa Show Material materials with Tensile strength of 585 - 724 MPa | Heat-Treated | ASTM A738 | Plate |
Yield strength | 485 MPa Show Material materials with Yield strength of 485 MPa | Heat-Treated | ASTM A738 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | Heat-Treated | ASTM A738 | Plate |
Boron | 0.0007 % Show Material materials with Boron of 0.0007 % | Heat-Treated | ASTM A738 | Plate |
Carbon | 0.1 % Show Material materials with Carbon of 0.1 % | Heat-Treated | ASTM A738 | Plate |
Chromium | 0.25 % Show Material materials with Chromium of 0.25 % | Heat-Treated | ASTM A738 | Plate |
Copper | 0.35 % Show Material materials with Copper of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Manganese | 1 - 1.6 % Show Material materials with Manganese of 1 - 1.6 % | Heat-Treated | ASTM A738 | Plate |
Molybdenum | 0.3 % Show Material materials with Molybdenum of 0.3 % | Heat-Treated | ASTM A738 | Plate |
Nickel | 0.6 % Show Material materials with Nickel of 0.6 % | Heat-Treated | ASTM A738 | Plate |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | Heat-Treated | ASTM A738 | Plate |
Phosphorus | 0.015 % Show Material materials with Phosphorus of 0.015 % | Heat-Treated | ASTM A738 | Plate |
Silicon | 0.15 - 0.5 % Show Material materials with Silicon of 0.15 - 0.5 % | Heat-Treated | ASTM A738 | Plate |
Sulfur | 0.006 % Show Material materials with Sulfur of 0.006 % | Heat-Treated | ASTM A738 | Plate |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % | Heat-Treated | ASTM A738 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |