ASTM A289 Grade 2 Stress Relieved

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Charpy impact energy

23.0 °C

88 J

Show Material materials with Charpy impact energy of 88 J

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation A50

23.0 °C

23 - 25 %

Show Material materials with Elongation A50 of 23 - 25 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Reduction of area

23.0 °C

55 - 58 %

Show Material materials with Reduction of area of 55 - 58 %

Tensile strength

23.0 °C

860 - 1070 MPa

Show Material materials with Tensile strength of 860 - 1070 MPa

Yield strength Rp0.2

23.0 °C

830 - 1000 MPa

Show Material materials with Yield strength Rp0.2 of 830 - 1000 MPa

Chemical properties

PropertyValue

Aluminium

0.04 %

Show Material materials with Aluminium of 0.04 %

Carbon

0.1 %

Show Material materials with Carbon of 0.1 %

Chromium

17.5 - 20 %

Show Material materials with Chromium of 17.5 - 20 %

Manganese

17.5 - 20 %

Show Material materials with Manganese of 17.5 - 20 %

Nickel

2 %

Show Material materials with Nickel of 2 %

Nitrogen

0.45 - 0.8 %

Show Material materials with Nitrogen of 0.45 - 0.8 %

Phosphorus

0.06 %

Show Material materials with Phosphorus of 0.06 %

Silicon

0.8 %

Show Material materials with Silicon of 0.8 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

Vanadium

0.25 %

Show Material materials with Vanadium of 0.25 %