General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 34 J Show Material materials with Charpy impact energy of 34 J | |
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 48 % Show Material materials with Reduction of area of 48 % | |
Tensile strength | 23.0 °C | 620 MPa Show Material materials with Tensile strength of 620 MPa | |
Yield strength | 23.0 °C | 485 MPa Show Material materials with Yield strength of 485 MPa | |
Yield strength Rp0.02 | 23.0 °C | 485 MPa Show Material materials with Yield strength Rp0.02 of 485 MPa | |
Yield strength Rp0.2 | 23.0 °C | 520 MPa Show Material materials with Yield strength Rp0.2 of 520 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.015 % Show Material materials with Aluminium of 0.015 % |
Carbon | 0.22 - 0.3 % Show Material materials with Carbon of 0.22 - 0.3 % |
Chromium | 0.75 % Show Material materials with Chromium of 0.75 % |
Manganese | 0.2 - 0.6 % Show Material materials with Manganese of 0.2 - 0.6 % |
Molybdenum | 0.4 - 0.6 % Show Material materials with Molybdenum of 0.4 - 0.6 % |
Nickel | 3.2 - 3.7 % Show Material materials with Nickel of 3.2 - 3.7 % |
Phosphorus | 0.01 % Show Material materials with Phosphorus of 0.01 % |
Sulfur | 0.012 % Show Material materials with Sulfur of 0.012 % |
Vanadium | 0.04 - 0.12 % Show Material materials with Vanadium of 0.04 - 0.12 % |