General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 16 % Show Material materials with Elongation A50 of 16 % | |
Hardness, Brinell | 23.0 °C | 248 [-] Show Material materials with Hardness, Brinell of 248 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 23.0 °C | 795 - 965 MPa Show Material materials with Tensile strength of 795 - 965 MPa | |
Yield strength Rp0.2 | 23.0 °C | 690 MPa Show Material materials with Yield strength Rp0.2 of 690 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.35 % Show Material materials with Carbon of 0.35 % |
Chromium | 0.8 - 2 % Show Material materials with Chromium of 0.8 - 2 % |
Manganese | 0.9 % Show Material materials with Manganese of 0.9 % |
Molybdenum | 0.2 - 0.4 % Show Material materials with Molybdenum of 0.2 - 0.4 % |
Nickel | 1.5 - 2.25 % Show Material materials with Nickel of 1.5 - 2.25 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.35 % Show Material materials with Silicon of 0.35 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Vanadium | 0.2 % Show Material materials with Vanadium of 0.2 % |