General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Density of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 220 GPa Show Material materials with Elastic modulus of 220 GPa | Typical for Martensitic Stainless Steel |
Elongation A50 | 20.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Poisson's ratio | 20.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Martensitic Stainless Steel |
Reduction of area | 20.0 °C | 35 % Show Material materials with Reduction of area of 35 % | |
Tensile strength | 20.0 °C | 585 - 760 MPa Show Material materials with Tensile strength of 585 - 760 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 415 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 415 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Melting point | 1375 - 1450 °C Show Material materials with Melting point of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Specific heat capacity | 20.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Thermal conductivity | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Thermal conductivity of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 20.0 °C | 6E-7 Ω·m Show Material materials with Electrical resistivity of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.03 % Show Material materials with Aluminium of 0.03 % |
Boron | 3E-3 % Show Material materials with Boron of 3E-3 % |
Calcium | 0.02 % Show Material materials with Calcium of 0.02 % |
Carbon | 0.28 - 0.33 % Show Material materials with Carbon of 0.28 - 0.33 % |
Chromium | 0.7 - 1 % Show Material materials with Chromium of 0.7 - 1 % |
Copper | 0.25 % Show Material materials with Copper of 0.25 % |
Manganese | 0.75 - 1.15 % Show Material materials with Manganese of 0.75 - 1.15 % |
Molybdenum | 0.3 - 0.45 % Show Material materials with Molybdenum of 0.3 - 0.45 % |
Nickel | 0.75 - 0.95 % Show Material materials with Nickel of 0.75 - 0.95 % |
Niobium | 0.01 % Show Material materials with Niobium of 0.01 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.35 % Show Material materials with Silicon of 0.35 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Titanium | 0.02 % Show Material materials with Titanium of 0.02 % |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % |