Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 0 - 20 % Show Material materials with Elongation A50 of 0 - 20 % |
Reduction of area | 20.0 °C | 0 - 48 % Show Material materials with Reduction of area of 0 - 48 % |
Tensile strength | 20.0 °C | 620 - 795 MPa Show Material materials with Tensile strength of 620 - 795 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 485 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 485 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 0.03 % Show Material materials with Aluminium of 0 - 0.03 % |
Boron | 0 - 3E-3 % Show Material materials with Boron of 0 - 3E-3 % |
Calcium | 0 - 0.02 % Show Material materials with Calcium of 0 - 0.02 % |
Carbon | 0.11 - 0.15 % Show Material materials with Carbon of 0.11 - 0.15 % |
Chromium | 2 - 2.5 % Show Material materials with Chromium of 2 - 2.5 % |
Copper | 0 - 0.25 % Show Material materials with Copper of 0 - 0.25 % |
Manganese | 0.3 - 0.6 % Show Material materials with Manganese of 0.3 - 0.6 % |
Molybdenum | 0.9 - 1.1 % Show Material materials with Molybdenum of 0.9 - 1.1 % |
Nickel | 0 - 0.25 % Show Material materials with Nickel of 0 - 0.25 % |
Niobium | 0 - 0.01 % Show Material materials with Niobium of 0 - 0.01 % |
Phosphorus | 0 - 0.02 % Show Material materials with Phosphorus of 0 - 0.02 % |
Silicon | 0 - 0.35 % Show Material materials with Silicon of 0 - 0.35 % |
Sulfur | 0 - 0.015 % Show Material materials with Sulfur of 0 - 0.015 % |
Titanium | 0 - 0.02 % Show Material materials with Titanium of 0 - 0.02 % |
Vanadium | 0 - 0.02 % Show Material materials with Vanadium of 0 - 0.02 % |