Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 23.0 °C | 20 J Show Material materials with Charpy impact energy of 20 J |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % |
Reduction of area | 23.0 °C | 38 % Show Material materials with Reduction of area of 38 % |
Tensile strength | 23.0 °C | 485 - 655 MPa Show Material materials with Tensile strength of 485 - 655 MPa |
Yield strength Rp0.2 | 23.0 °C | 250 MPa Show Material materials with Yield strength Rp0.2 of 250 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.35 % Show Material materials with Carbon of 0.35 % |
Chromium | 0.25 % Show Material materials with Chromium of 0.25 % |
Manganese | 0.4 - 0.9 % Show Material materials with Manganese of 0.4 - 0.9 % |
Molybdenum | 0.1 % Show Material materials with Molybdenum of 0.1 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.35 % Show Material materials with Silicon of 0.35 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % |