General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 20.0 °C | 60 J Show Material materials with Charpy impact energy of 60 J | |
Elastic modulus | 20.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Nickel Molybdenum Steel |
Elongation | 20.0 °C | 12 % Show Material materials with Elongation of 12 % | |
Poisson's ratio | 20.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Reduction of area | 20.0 °C | 36 % Show Material materials with Reduction of area of 36 % | |
Tensile strength | 20.0 °C | 1210 MPa Show Material materials with Tensile strength of 1210 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1100 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1100 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 9E-6 - 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 9E-6 - 1.3E-5 1/K | Typical for Nickel Molybdenum Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel | |
Thermal conductivity | 20.0 °C | 44 W/(m·K) Show Material materials with Thermal conductivity of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.23 - 0.28 % Show Material materials with Carbon of 0.23 - 0.28 % |
Chromium | 1.4 - 1.65 % Show Material materials with Chromium of 1.4 - 1.65 % |
Manganese | 0.2 % Show Material materials with Manganese of 0.2 % |
Molybdenum | 0.8 - 1 % Show Material materials with Molybdenum of 0.8 - 1 % |
Nickel | 2.75 - 3.25 % Show Material materials with Nickel of 2.75 - 3.25 % |
Phosphorus | 0.01 % Show Material materials with Phosphorus of 0.01 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |