Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 20.0 °C | 17 J Show Material materials with Charpy impact energy of 17 J |
Elongation | 20.0 °C | 6 % Show Material materials with Elongation of 6 % |
Reduction of area | 20.0 °C | 25 % Show Material materials with Reduction of area of 25 % |
Tensile strength | 20.0 °C | 1720 MPa Show Material materials with Tensile strength of 1720 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1550 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1550 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.4 - 0.45 % Show Material materials with Carbon of 0.4 - 0.45 % |
Chromium | 0.65 - 0.9 % Show Material materials with Chromium of 0.65 - 0.9 % |
Manganese | 0.65 - 0.9 % Show Material materials with Manganese of 0.65 - 0.9 % |
Molybdenum | 0.3 - 0.45 % Show Material materials with Molybdenum of 0.3 - 0.45 % |
Nickel | 1.65 - 2 % Show Material materials with Nickel of 1.65 - 2 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1.45 - 1.8 % Show Material materials with Silicon of 1.45 - 1.8 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |