Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 20.0 °C | 20 J Show Material materials with Charpy impact energy of 20 J |
Elongation | 20.0 °C | 6 % Show Material materials with Elongation of 6 % |
Reduction of area | 20.0 °C | 25 % Show Material materials with Reduction of area of 25 % |
Tensile strength | 20.0 °C | 1720 MPa Show Material materials with Tensile strength of 1720 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1550 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1550 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.41 - 0.46 % Show Material materials with Carbon of 0.41 - 0.46 % |
Chromium | 1.9 - 2.25 % Show Material materials with Chromium of 1.9 - 2.25 % |
Manganese | 0.75 - 1 % Show Material materials with Manganese of 0.75 - 1 % |
Molybdenum | 0.45 - 0.6 % Show Material materials with Molybdenum of 0.45 - 0.6 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1.4 - 1.75 % Show Material materials with Silicon of 1.4 - 1.75 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Vanadium | 0.03 - 0.08 % Show Material materials with Vanadium of 0.03 - 0.08 % |