Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 20.0 °C | 20 J Show Material materials with Charpy impact energy of 20 J |
Elongation | 20.0 °C | 8 - 9 % Show Material materials with Elongation of 8 - 9 % |
Reduction of area | 20.0 °C | 25 - 30 % Show Material materials with Reduction of area of 25 - 30 % |
Tensile strength | 20.0 °C | 1790 - 1930 MPa Show Material materials with Tensile strength of 1790 - 1930 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1380 - 1550 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1380 - 1550 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.38 - 0.43 % Show Material materials with Carbon of 0.38 - 0.43 % |
Chromium | 4.75 - 5.25 % Show Material materials with Chromium of 4.75 - 5.25 % |
Manganese | 0.2 - 0.4 % Show Material materials with Manganese of 0.2 - 0.4 % |
Molybdenum | 1.2 - 1.4 % Show Material materials with Molybdenum of 1.2 - 1.4 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.8 - 1 % Show Material materials with Silicon of 0.8 - 1 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Vanadium | 0.4 - 0.6 % Show Material materials with Vanadium of 0.4 - 0.6 % |