ASTM A579 Grade 73 Type 7, Maraging

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Nickel Molybdenum Steel

Mechanical

PropertyTemperatureValueComment

Charpy impact energy

20.0 °C

20 J

Show Material materials with Charpy impact energy of 20 J

Elastic modulus

20.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Nickel Molybdenum Steel

Elongation

20.0 °C

9 %

Show Material materials with Elongation of 9 %

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Nickel Molybdenum Steel

Reduction of area

20.0 °C

40 %

Show Material materials with Reduction of area of 40 %

Tensile strength

20.0 °C

1930 MPa

Show Material materials with Tensile strength of 1930 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

1895 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 1895 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

9E-6 - 1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 9E-6 - 1.3E-5 1/K

Typical for Nickel Molybdenum Steel

Melting point

1382 - 1529 °C

Show Material materials with Melting point of 1382 - 1529 °C

Typical for Nickel Molybdenum Steel

Thermal conductivity

20.0 °C

44 W/(m·K)

Show Material materials with Thermal conductivity of 44 W/(m·K)

Typical for Nickel Molybdenum Steel

Chemical properties

PropertyValue

Aluminium

0.05 - 0.15 %

Show Material materials with Aluminium of 0.05 - 0.15 %

Carbon

0.03 %

Show Material materials with Carbon of 0.03 %

Cobalt

8.5 - 9.5 %

Show Material materials with Cobalt of 8.5 - 9.5 %

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Molybdenum

4.6 - 5.2 %

Show Material materials with Molybdenum of 4.6 - 5.2 %

Nickel

18 - 19 %

Show Material materials with Nickel of 18 - 19 %

Phosphorus

0.01 %

Show Material materials with Phosphorus of 0.01 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %

Titanium

0.5 - 0.8 %