General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 45 J Show Material materials with Charpy impact energy of 45 J | |
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation | 23.0 °C | 12 % Show Material materials with Elongation of 12 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 55 % Show Material materials with Reduction of area of 55 % | |
Tensile strength | 23.0 °C | 1450 MPa Show Material materials with Tensile strength of 1450 MPa | |
Yield strength Rp0.2 | 23.0 °C | 1380 MPa Show Material materials with Yield strength Rp0.2 of 1380 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 - 0.15 % Show Material materials with Aluminium of 0.05 - 0.15 % |
Carbon | 0.03 % Show Material materials with Carbon of 0.03 % |
Cobalt | 8 - 9 % Show Material materials with Cobalt of 8 - 9 % |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % |
Molybdenum | 3 - 3.5 % Show Material materials with Molybdenum of 3 - 3.5 % |
Nickel | 17 - 19 % Show Material materials with Nickel of 17 - 19 % |
Phosphorus | 0.01 % Show Material materials with Phosphorus of 0.01 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |
Titanium | 0.15 - 0.25 % Show Material materials with Titanium of 0.15 - 0.25 % |