General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 25 J Show Material materials with Charpy impact energy of 25 J | |
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation | 23.0 °C | 10 % Show Material materials with Elongation of 10 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 30 % Show Material materials with Reduction of area of 30 % | |
Tensile strength | 23.0 °C | 1450 MPa Show Material materials with Tensile strength of 1450 MPa | |
Yield strength Rp0.2 | 23.0 °C | 1380 MPa Show Material materials with Yield strength Rp0.2 of 1380 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.28 - 0.34 % Show Material materials with Carbon of 0.28 - 0.34 % |
Chromium | 0.9 - 1.1 % Show Material materials with Chromium of 0.9 - 1.1 % |
Cobalt | 4 - 5 % Show Material materials with Cobalt of 4 - 5 % |
Manganese | 0.1 - 0.35 % Show Material materials with Manganese of 0.1 - 0.35 % |
Molybdenum | 0.9 - 1.1 % Show Material materials with Molybdenum of 0.9 - 1.1 % |
Nickel | 7 - 8.5 % Show Material materials with Nickel of 7 - 8.5 % |
Phosphorus | 0.01 % Show Material materials with Phosphorus of 0.01 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |
Vanadium | 0.06 - 0.12 % Show Material materials with Vanadium of 0.06 - 0.12 % |