General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Elongation A50 | 20.0 °C | 12 % Show Material materials with Elongation A50 of 12 % | |
Poisson's ratio | 20.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Reduction of area | 20.0 °C | 30 % Show Material materials with Reduction of area of 30 % | |
Tensile strength | 20.0 °C | 1030 MPa Show Material materials with Tensile strength of 1030 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 890 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 890 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Specific heat capacity | 20.0 °C | 448 - 502 J/(kg·K) Show Material materials with Specific heat capacity of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Thermal conductivity | 20.0 °C | 36 - 43 W/(m·K) Show Material materials with Thermal conductivity of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.45 - 0.6 % Show Material materials with Carbon of 0.45 - 0.6 % |
Chromium | 0.8 - 1.15 % Show Material materials with Chromium of 0.8 - 1.15 % |
Manganese | 0.55 - 1.05 % Show Material materials with Manganese of 0.55 - 1.05 % |
Molybdenum | 0.15 - 0.5 % Show Material materials with Molybdenum of 0.15 - 0.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |