Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.72 - 8 g/cm³ Show Material materials with Density of 7.72 - 8 g/cm³ | Typical for Tool And Machining Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 203 - 211 GPa Show Material materials with Elastic modulus of 203 - 211 GPa | Typical for Tool And Machining Steel |
Hardness, Brinell | 23.0 °C | 262 [-] Show Material materials with Hardness, Brinell of 262 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Tool And Machining Steel |
Shear modulus | 23.0 °C | 79 GPa Show Material materials with Shear modulus of 79 GPa | Typical for Tool And Machining Steel |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K | Typical for Tool And Machining Steel |
Melting point | 1370 - 1425 °C Show Material materials with Melting point of 1370 - 1425 °C | Typical for Tool And Machining Steel | |
Specific heat capacity | 23.0 °C | 420 - 460 J/(kg·K) Show Material materials with Specific heat capacity of 420 - 460 J/(kg·K) | Typical for Tool And Machining Steel |
Thermal conductivity | 23.0 °C | 17 - 42 W/(m·K) Show Material materials with Thermal conductivity of 17 - 42 W/(m·K) | Typical for Tool And Machining Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.5 - 0.65 % Show Material materials with Carbon of 0.5 - 0.65 % |
Chromium | 3.75 - 4.5 % Show Material materials with Chromium of 3.75 - 4.5 % |
Manganese | 0.15 - 0.4 % Show Material materials with Manganese of 0.15 - 0.4 % |
Molybdenum | 7.75 - 8.5 % Show Material materials with Molybdenum of 7.75 - 8.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.2 - 0.45 % Show Material materials with Silicon of 0.2 - 0.45 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |
Vanadium | 1.8 - 2.2 % Show Material materials with Vanadium of 1.8 - 2.2 % |