ASTM A681 Grade Type A7 Annealed

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

Mechanical

Hardness, Brinell HB

269 [-] at 20 °C

Thermal

Coefficient of thermal expansion α

1E-5 - 1.3E-5 1/K at 20 °C

Typical for Tool And Machining Steel

Melting point Tm

1370 - 1425 °C

Typical for Tool And Machining Steel

Specific heat capacity cp

420 - 460 J/(kg·K) at 20 °C

Typical for Tool And Machining Steel

Thermal conductivity λ

17 - 42 W/(m·K) at 20 °C

Typical for Tool And Machining Steel

Chemical properties

Element

Weight %

Comment

Cr

5 - 5.75 %

V

3.9 - 5.15 %

C

2 - 2.85 %

Mo

0.9 - 1.4 %

W

0.5 - 1.5 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.