Hardness, Brinell HB
0 - 241 [-] at 20 °C
Melting point Tm
1370 - 1425 °C
Typical for Tool And Machining Steel
Specific heat capacity cp
420 - 460 J/(kg·K) at 20 °C
Typical for Tool And Machining Steel
Thermal conductivity λ
17 - 42 W/(m·K) at 20 °C
Typical for Tool And Machining Steel
Element
Weight %
Comment
1.3 - 1.7 %
0.95 - 1.1 %
0.25 - 0.8 %
0.1 - 0.5 %
0.1 - 0.3 %
This material data has been provided by ASTM.