General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Hardness, Brinell | 23.0 °C | 255 [-] Show Material materials with Hardness, Brinell of 255 [-] | |
Hardness, Rockwell B | 23.0 °C | 100 [-] Show Material materials with Hardness, Rockwell B of 100 [-] | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Specific heat capacity | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Specific heat capacity of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Thermal conductivity | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Thermal conductivity of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Carbon | 0.95 - 1.2 % Show Material materials with Carbon of 0.95 - 1.2 % |
Chromium | 16 - 18 % Show Material materials with Chromium of 16 - 18 % |
Copper | 0.5 % Show Material materials with Copper of 0.5 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 0.4 - 0.65 % Show Material materials with Molybdenum of 0.4 - 0.65 % |
Nickel | 0.75 % Show Material materials with Nickel of 0.75 % |
Oxygen | 2E-3 % Show Material materials with Oxygen of 2E-3 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |