Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 20.0 °C | 20 J Show Material materials with Charpy impact energy of 20 J | |
Elastic modulus | 20.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Low Carbon Steel |
Elongation A50 | 20.0 °C | 22 % Show Material materials with Elongation A50 of 22 % | |
Poisson's ratio | 20.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Low Carbon Steel |
Reduction of area | 20.0 °C | 35 % Show Material materials with Reduction of area of 35 % | |
Shear modulus | 20.0 °C | 75 - 80 GPa Show Material materials with Shear modulus of 75 - 80 GPa | Typical for Carbon Steel |
Tensile strength | 20.0 °C | 485 - 655 MPa Show Material materials with Tensile strength of 485 - 655 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 260 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 260 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Max service temperature | 500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1480 - 1526 °C Show Material materials with Melting point of 1480 - 1526 °C | Typical for Low Carbon Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnetic
Property | Temperature | Value | Comment |
---|---|---|---|
Curie temperature | 20.0 °C | 770 °C Show Material materials with Curie temperature of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Carbon | 0.2 % Show Material materials with Carbon of 0.2 % |
Chromium | 0.2 % Show Material materials with Chromium of 0.2 % |
Copper | 0.35 % Show Material materials with Copper of 0.35 % |
Manganese | 0.9 % Show Material materials with Manganese of 0.9 % |
Molybdenum | 0.06 % Show Material materials with Molybdenum of 0.06 % |
Nickel | 3.3 - 3.8 % Show Material materials with Nickel of 3.3 - 3.8 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % |