General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A200 | 23.0 °C | 16 % Show Material materials with Elongation A200 of 16 % | |
Elongation A50 | 23.0 °C | 18 % Show Material materials with Elongation A50 of 18 % | |
Hardness, Brinell | 23.0 °C | 167 [-] Show Material materials with Hardness, Brinell of 167 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 23.0 °C | 515 MPa Show Material materials with Tensile strength of 515 MPa | |
Yield strength | 23.0 °C | 415 MPa Show Material materials with Yield strength of 415 MPa |
Chemical properties
Property | Value |
---|---|
Molybdenum | 0.01 - 0.3 % Show Material materials with Molybdenum of 0.01 - 0.3 % |
Niobium | 0.01 - 0.07 % Show Material materials with Niobium of 0.01 - 0.07 % |
Titanium | 0.03 % Show Material materials with Titanium of 0.03 % |
Vanadium | 0.02 - 0.2 % Show Material materials with Vanadium of 0.02 - 0.2 % |