Mechanical

PropertyValueTemperature

Elongation A50

0 - 5 %

Show Material materials with Elongation A50 of 0 - 5 % at 20.0 °C

20.0 °C

Tensile strength

0 - 485 MPa

Show Material materials with Tensile strength of 0 - 485 MPa at 20.0 °C

20.0 °C

Yield strength

0 - 345 MPa

Show Material materials with Yield strength of 0 - 345 MPa at 20.0 °C

20.0 °C