General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A200 | 23.0 °C | 13 % Show Material materials with Elongation A200 of 13 % | |
Elongation A50 | 23.0 °C | 17 % Show Material materials with Elongation A50 of 17 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 23.0 °C | 550 MPa Show Material materials with Tensile strength of 550 MPa | |
Yield strength Rp0.5 | 23.0 °C | 305 MPa Show Material materials with Yield strength Rp0.5 of 305 MPa |