General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Duplex Stainless Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 200 GPa Show Material materials with Elastic modulus of 200 GPa | Typical for Duplex Stainless Steel |
Elongation A50 | 20.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Poisson's ratio | 20.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Duplex Stainless Steel |
Tensile strength | 20.0 °C | 455 MPa Show Material materials with Tensile strength of 455 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 360 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 360 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 1/K | Typical for Duplex Stainless Steel |
Max service temperature | 300 °C Show Material materials with Max service temperature of 300 °C | Typical for Duplex Stainless Steel | |
Melting point | 1375 - 1450 °C Show Material materials with Melting point of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Specific heat capacity | 20.0 °C | 440 - 502 J/(kg·K) Show Material materials with Specific heat capacity of 440 - 502 J/(kg·K) | Typical for Duplex Stainless Steel |
Thermal conductivity | 20.0 °C | 13 - 30 W/(m·K) Show Material materials with Thermal conductivity of 13 - 30 W/(m·K) | Typical for Duplex Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.3 % Show Material materials with Carbon of 0.3 % |
Manganese | 1.6 % Show Material materials with Manganese of 1.6 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |