General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A80 | 20.0 °C | 12 % Show Material materials with Elongation A80 of 12 % | |
Hardness, Brinell | 20.0 °C | 96 [-] Show Material materials with Hardness, Brinell of 96 [-] | |
Hardness, Vickers | 20.0 °C | 230 [-] Show Material materials with Hardness, Vickers of 230 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 20.0 °C | 740 MPa Show Material materials with Tensile strength of 740 MPa | |
Yield strength Rp0.2 | 20.0 °C | 600 MPa Show Material materials with Yield strength Rp0.2 of 600 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.52 - 0.6 % Show Material materials with Carbon of 0.52 - 0.6 % |
Chromium | 0.4 % Show Material materials with Chromium of 0.4 % |
Manganese | 0.6 - 0.9 % Show Material materials with Manganese of 0.6 - 0.9 % |
Molybdenum | 0.1 % Show Material materials with Molybdenum of 0.1 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1.6 - 2 % Show Material materials with Silicon of 1.6 - 2 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Do you have a technical question or need more information about this material?