General
Property | Value | Comment |
---|---|---|
Density | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Low Carbon Steel | |||
Elongation | 10.1 % Show Material materials with Elongation of 10.1 % | Predicted Value, A200 | |||
16.2 % Show Material materials with Elongation of 16.2 % | Predicted Value, A80 | ||||
19 % Show Material materials with Elongation of 19 % | Quenched and Tempered | ASTM A709 | Plate, Bar | A50 | |
19.6 % Show Material materials with Elongation of 19.6 % | Predicted Value, A80 Transverse | ||||
20.5 % Show Material materials with Elongation of 20.5 % | Predicted Value, Transverse | ||||
22.8 % Show Material materials with Elongation of 22.8 % | Predicted Value | ||||
Poisson's ratio | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Low Carbon Steel | |||
Reduction of area | 42.9 % Show Material materials with Reduction of area of 42.9 % | Predicted Value, Transverse | |||
45.7 % Show Material materials with Reduction of area of 45.7 % | Predicted Value | ||||
Shear modulus | 82 GPa Show Material materials with Shear modulus of 82 GPa | Typical for Low Carbon Steel | |||
Shear strength | 644.8 MPa Show Material materials with Shear strength of 644.8 MPa | Predicted Value | |||
Tensile strength | 585 - 760 MPa Show Material materials with Tensile strength of 585 - 760 MPa | Quenched and Tempered | ASTM A709 | Plate, Bar |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max service temperature | 326.5 °C Show Material materials with Max service temperature of 326.5 °C | Predicted Value, Long |
500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1480 - 1526 °C Show Material materials with Melting point of 1480 - 1526 °C | Typical for Low Carbon Steel |
Specific heat capacity | 465 J/(kg·K) Show Material materials with Specific heat capacity of 465 J/(kg·K) | Typical for Low Carbon Steel |
Thermal conductivity | 25 - 93 W/(m·K) Show Material materials with Thermal conductivity of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 8 S/m Show Material materials with Electrical conductivity of 8 S/m | Predicted Value |
Electrical resistivity | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetic
Property | Value | Comment |
---|---|---|
Curie temperature | 770 °C Show Material materials with Curie temperature of 770 °C | Typical for Low Carbon Steel |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |