General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 16 - 18 % Show Material materials with Elongation A50 of 16 - 18 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 23.0 °C | 690 - 895 MPa Show Material materials with Tensile strength of 690 - 895 MPa | |
Yield strength Rp0.2 | 23.0 °C | 620 - 690 MPa Show Material materials with Yield strength Rp0.2 of 620 - 690 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 - 0.05 % Show Material materials with Aluminium of 0.02 - 0.05 % |
Carbon | 0.08 % Show Material materials with Carbon of 0.08 % |
Chromium | 0.4 - 0.65 % Show Material materials with Chromium of 0.4 - 0.65 % |
Copper | 0.9 - 1.2 % Show Material materials with Copper of 0.9 - 1.2 % |
Manganese | 0.95 - 1.5 % Show Material materials with Manganese of 0.95 - 1.5 % |
Molybdenum | 0.4 - 0.65 % Show Material materials with Molybdenum of 0.4 - 0.65 % |
Nickel | 0.65 - 0.9 % Show Material materials with Nickel of 0.65 - 0.9 % |
Niobium | 0.01 - 0.03 % Show Material materials with Niobium of 0.01 - 0.03 % |
Nitrogen | 0.02 % Show Material materials with Nitrogen of 0.02 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % |
Sulfur | 6E-3 % Show Material materials with Sulfur of 6E-3 % |