ASTM A414 Grade B Hot-Rolled

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A200

23.0 °C

18 %

Show Material materials with Elongation A200 of 18 %

Elongation A50

23.0 °C

21 - 24 %

Show Material materials with Elongation A50 of 21 - 24 %

Tensile strength

23.0 °C

345 - 450 MPa

Show Material materials with Tensile strength of 345 - 450 MPa

Yield strength

23.0 °C

205 MPa

Show Material materials with Yield strength of 205 MPa

Chemical properties

PropertyValue

Aluminium

0.02 - 0.08 %

Show Material materials with Aluminium of 0.02 - 0.08 %

Carbon

0.22 %

Show Material materials with Carbon of 0.22 %

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

Copper

0.4 %

Show Material materials with Copper of 0.4 %

Manganese

0.9 %

Show Material materials with Manganese of 0.9 %

Molybdenum

0.12 %

Show Material materials with Molybdenum of 0.12 %

Nickel

0.4 %

Show Material materials with Nickel of 0.4 %

Niobium

0.02 %

Show Material materials with Niobium of 0.02 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %

Titanium

0.03 %

Show Material materials with Titanium of 0.03 %

Vanadium

0.03 %

Show Material materials with Vanadium of 0.03 %