General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 20 - 27 J Show Material materials with Charpy impact energy of 20 - 27 J | |
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Tensile strength | 23.0 °C | 620 MPa Show Material materials with Tensile strength of 620 MPa | |
Yield strength Rp0.2 | 23.0 °C | 550 - 585 MPa Show Material materials with Yield strength Rp0.2 of 550 - 585 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel | |
Specific heat capacity | 23.0 °C | 448 - 670 J/(kg·K) Show Material materials with Specific heat capacity of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity | 23.0 °C | 34 - 54 W/(m·K) Show Material materials with Thermal conductivity of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |