ASTM A479 Grade 316 Strain-Hardened level 1

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperatureComment

Density

7.9 - 8.2 g/cm³

Show Material materials with Density of 7.9 - 8.2 g/cm³ at 23.0 °C

23.0 °C

Typical for Austenitic Stainless Steel

Mechanical

PropertyValueTemperatureComment

Elastic modulus

195 GPa

Show Material materials with Elastic modulus of 195 GPa at 23.0 °C

23.0 °C

Typical for Austenitic Stainless Steel

Elongation A50

30 %

Show Material materials with Elongation A50 of 30 % at 23.0 °C

23.0 °C

Poisson's ratio

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-] at 23.0 °C

23.0 °C

Typical for Austenitic Stainless Steel

Reduction of area

60 %

Show Material materials with Reduction of area of 60 % at 23.0 °C

23.0 °C

Shear modulus

77 GPa

Show Material materials with Shear modulus of 77 GPa at 23.0 °C

23.0 °C

Typical for Austenitic Stainless Steel

Tensile strength

585 MPa

Show Material materials with Tensile strength of 585 MPa at 23.0 °C

23.0 °C

Yield strength Rp0.2

450 MPa

Show Material materials with Yield strength Rp0.2 of 450 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

1.7E-5 - 1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K at 23.0 °C

23.0 °C

Typical for Austenitic Stainless Steel

Melting point

1230 - 1480 °C

Show Material materials with Melting point of 1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

440 J/(kg·K)

Show Material materials with Specific heat capacity of 440 J/(kg·K) at 23.0 °C

23.0 °C

Typical for Austenitic Stainless Steel

Thermal conductivity

11 - 21 W/(m·K)

Show Material materials with Thermal conductivity of 11 - 21 W/(m·K) at 23.0 °C

23.0 °C

Typical for Austenitic Stainless Steel

Electrical

PropertyValueTemperatureComment

Electrical resistivity

8.5E-7 Ω·m

Show Material materials with Electrical resistivity of 8.5E-7 Ω·m at 23.0 °C

23.0 °C

Typical for Austenitic Stainless Steel

Chemical properties

Property

Carbon

0.08 %

Chromium

16 - 18 %

Manganese

2 %

Molybdenum

2 - 3 %

Nickel

10 - 14 %

Phosphorus

0.05 %

Silicon

1 %

Sulfur

0.03 %