Reduction of area Z
40 % at 20 °C
Tensile strength Rm
515 MPa at 20 °C
Yield strength YS
205 MPa at 20 °C
Element
Weight %
Comment
63.63 - 73.96 %
17 - 19 %
9 - 13 %
0.04 - 0.1 %
0 - 0.03 %
Processing history
annealed
This material data has been provided by MetalInfo.